Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 110.94 MPa @Strain 1.22 %, Temperature 0.000 °C |
16091 psi @Strain 1.22 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9030FR NC010 PBT+ASA
(Unverified Data**) 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030FR NC010 is a 30% glass fiber reinforced flame retardant polybutylene terephthal.. |