Polymer Property : Tensile Stress = 15800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 109 MPa

@Strain 3.00 %,
Temperature 0.000 °C
15800 psi

@Strain 3.00 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® 415HP NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
15% Glass Reinforced Polyethylene Terephthalate with Excellent Impact Resistance Rynite 415HP NC010 is a 15% glass reinforced modified polyethylene terephthalate improved for easy fast processing ov..
Tensile Stress 109 MPa

@Strain 1.68 %,
Temperature 0.000 °C
15800 psi

@Strain 1.68 %,
Temperature 32.0 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Minlon® EFE6053 BK413 Nylon 66  (Unverified Data**)
40% Mineral/Glass Reinforced Polyamide 66 Minlon EFE6053 BK413 is a 40% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance P..
Tensile Stress 109 MPa

@Strain 0.844 %,
Temperature 23.0 °C
15800 psi

@Strain 0.844 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 73G45L NC010 Nylon 6  (Unverified Data**)
45% Glass Reinforced Polyamide 6Zytel 73G45L NC010 is a 45% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers