Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 10.8 MPa @Strain 1.10 %, Temperature 90.0 °C |
1570 psi @Strain 1.10 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100P NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer with Improved Processing Delrin 100P is a high viscosity acetal homopolymer for use in easy to fill molds. It has improved processing thermal stability good mechani.. |
|||
Tensile Stress | 10.8 MPa @Strain 1.10 %, Temperature 90.0 °C |
1570 psi @Strain 1.10 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG100P NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG100P is a high viscosity acetal homopolymer with improved thermal stability for use in easy to fill molds. It has b.. |
|||
Tensile Stress | 10.8 MPa @Strain 132.12 %, Temperature 120 °C |
1570 psi @Strain 132.12 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® RS R4275 BK316 Polyester Elastomer TPC-ET 55 Shore D Renewably Sourced High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 10.8 MPa @Strain 300 % |
1570 psi @Strain 300 % |
ISO 37 |
Alliance Polymers Viprene™ G40D-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G40D-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 10.8 MPa @Strain 300 % |
1570 psi @Strain 300 % |
ISO 37 |
Alliance Polymers Viprene™ G40D-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G40D-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |