Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 10.76 MPa @Strain 187.76 %, Temperature 90.0 °C |
1561 psi @Strain 187.76 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® DYM350BK TPC-ET+PBT
(Unverified Data**) Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 10.76 MPa @Strain 52.81 %, Temperature 90.0 °C |
1561 psi @Strain 52.81 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® RS R4275 BK316 Polyester Elastomer TPC-ET 55 Shore D Renewably Sourced High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Information provided by DuPont Performance Polymers |