Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 10.61 MPa @Strain 2.43 %, Temperature 90.0 °C |
1539 psi @Strain 2.43 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® S620F20 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin S620F20 NC010 is an unreinforced nucleated lubricated medium viscosity polybutylene terephthalate resin for fast injection molding.In.. |
|||
Tensile Stress | 10.61 MPa @Strain 216.08 %, Temperature 100 °C |
1539 psi @Strain 216.08 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® DYM350BK TPC-ET+PBT
(Unverified Data**) Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsInformation provided by DuPont Performance Polymers |