Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 105.35 MPa @Strain 1.73 %, Temperature 0.000 °C |
15280 psi @Strain 1.73 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9320 NC010 PBT+SAN
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9320 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. I.. |