Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 102 MPa @Strain 9.00 %, Temperature 120 °C |
14800 psi @Strain 9.00 %, Temperature 248 °F |
|
Solvay TECHNYL® A 218 V30 PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |