Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 101.18 MPa @Strain 3.43 %, Temperature 0.000 °C |
14675 psi @Strain 3.43 %, Temperature 32.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 73G15L NC010 Nylon 6