Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 10.1 MPa @Strain 100 % |
1460 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® D6895 TPE, Extruded Characteristics: Good melt strengthSoft touchSmooth surface with dry feelGood weather and heat resistanceWide range of hardnessEasy processingTypical Applications: IndustrialPackagingConsumerHeathca.. |
|||
Tensile Stress | 10.1 MPa @Strain 300 % |
1460 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® P3990H TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 10.1 MPa @Strain 14.98 %, Temperature 150 °C |
1460 psi @Strain 14.98 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN FE8200 NC010 Polyphthalamide (PPA)
(Unverified Data**) Unreinforced Toughened PPA High Performance Polyamide Zytel HTNFE8200 NC010 is an unreinforced toughened heat stabilized lubricated high performance polyamide resin for injection molding. It is also.. |
|||
Tensile Stress | 10.1 MPa @Strain 100 % |
1460 psi @Strain 100 % |
ISO 37 |
Alliance Polymers Viprene™ P55D-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P55D-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 10.1 MPa @Strain 100 % |
1460 psi @Strain 100 % |
ISO 37 |
Alliance Polymers Viprene™ P55D-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P55D-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 10.1 MPa @Strain 300 % |
1460 psi @Strain 300 % |
ISO 37 |
Alliance Polymers Viprene™ P90A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P90A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 10.1 MPa @Strain 300 % |
1460 psi @Strain 300 % |
ISO 37 |
Alliance Polymers Viprene™ P90A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P90A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |