Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 99.12 MPa @Strain 1.01 %, Temperature -40.0 °C |
14380 psi @Strain 1.01 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® HR5330HF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)& 30% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5330HF is a 30% glass reinforced PBT with high flow (HF) moderately toughened hydrolysis resistant (HR) resin. Excellen.. |
|||
Tensile Stress | 99.15 MPa @Strain 1.61 %, Temperature 0.000 °C |
14380 psi @Strain 1.61 %, Temperature 32.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® BM70G20HSLX BK537 Nylon 66
(Unverified Data**) 20% Glass Reinforced Heat Stabilized Polyamide 66 Developed for Blow Molding Zytel BM70G20HSLX BK537 is a 20% glass fiber reinforced polyamide 66 for blow molding.Information provided by DuPont Perf.. |