Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 98.64 MPa @Strain 0.870 %, Temperature 23.0 °C |
14310 psi @Strain 0.870 %, Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Crastin® SK608 BK509 PBT
(Unverified Data**) Crastin® SK608 BK509 is a 45% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 98.66 MPa @Strain 1.70 %, Temperature 40.0 °C |
14310 psi @Strain 1.70 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS 30G30L NC010 Nylon 610 30% Glass Reinforced Renewably Sourced Polyamide 610 Developed for Extrusion Zytel RS 30G30L NC010 is a lubricated 30% glass fiber reinforced polyamide 610 resin containing a minimum of 40% renewabl.. |