Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 98.25 MPa @Strain 0.940 %, Temperature -40.0 °C |
14250 psi @Strain 0.940 %, Temperature -40.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS 30G30L NC010 Nylon 610 30% Glass Reinforced Renewably Sourced Polyamide 610 Developed for Extrusion Zytel RS 30G30L NC010 is a lubricated 30% glass fiber reinforced polyamide 610 resin containing a minimum of 40% renewabl.. |