Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 94.37 MPa @Strain 3.60 %, Temperature 120 °C |
13690 psi @Strain 3.60 %, Temperature 248 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® 70G35HSLRA4 BK267 Nylon 66
(Unverified Data**) Zytel® 70G35HSLRA4 BK267 is a 35% glass fiber reinforced, heat stabilized, hydrolysis resistant polyamide 66 resin for injection molding. It has excellent flow characteristics.Information provided .. |
|||
Tensile Stress | 94.42 MPa @Strain 2.82 %, Temperature 40.0 °C |
13690 psi @Strain 2.82 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66
(Unverified Data**) 25% Glass Reinforced Flame Retardant Polyamide 66 Zytel FR70G25V0 NC010 is a 25% glass fiber reinforced heat stabilized flame retardant polyamide 66 resin for injection molding.Information provided .. |