Mechanical Properties Metric English Comments
Tensile Stress 13.68 MPa

@Strain 0.100 %,
Temperature -40.0 °C
1984 psi

@Strain 0.100 %,
Temperature -40.0 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS95G40DH1T BK261 Nylon  (Unverified Data**)
Zytel® PLS95G40DH1T is a 40% GR impact modified PA, made with SHIELD technology, its superior heat & oil resistance combined with the "stone impact resistance" makes it ideal choice for use in seve..