Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 88.88 MPa @Strain 2.47 %, Temperature 90.0 °C |
12890 psi @Strain 2.47 %, Temperature 194 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G35HSLRA4 BK267 Nylon 66
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Hydrolysis Resistant Polyamide 66 Zytel 70G35HSLRA4 BK267 is a 35% glass fiber reinforced heat stabilized hydrolysis resistant polyamide 66 resin for injection m.. |
|||
Tensile Stress | 88.89 MPa @Strain 2.62 %, Temperature 90.0 °C |
12890 psi @Strain 2.62 %, Temperature 194 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 51G35EF BK083 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide Developed for Electrical and Electronics Applications Zytel HTN51G35EF BK083 is a 35% glass reinforced heat stabilized lubricated high performance.. |
|||
Tensile Stress | 88.89 MPa @Strain 2.62 %, Temperature 90.0 °C |
12890 psi @Strain 2.62 %, Temperature 194 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 51G35HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G35HSL BK083 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information .. |