Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 88.69 MPa @Strain 0.900 %, Temperature 23.0 °C |
12860 psi @Strain 0.900 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 74G33W BK196 Nylon 66
(Unverified Data**) 33% Glass Reinforced UV Stabilized Polyamide 66 + Polyamide 6 Zytel 74G33W BK196 is a high gloss automotive weatherable black 33% glass reinforced nylon 66 and nylon 6 comelt resin.Information provi.. |
|||
Tensile Stress | 88.65 MPa @Strain 3.49 %, Temperature 90.0 °C |
12860 psi @Strain 3.49 %, Temperature 194 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® PLS 93G35DH1 BK549 Nylon 6
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 6 Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 88.69 MPa @Strain 5.16 %, Temperature -20.0 °C |
12860 psi @Strain 5.16 %, Temperature -4.00 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 73M30 NC010 Nylon 6
(Unverified Data**) 30% Mineral Reinforced Polyamide 6 Minlon 73M30 NC010 is a 30% mineral reinforced heat stabilized polyamide 6 resin for injection molding. It has isotropic properties and low warpage.Information pro.. |
|||
Tensile Stress | 88.64 MPa @Strain 3.44 %, Temperature 23.0 °C |
12860 psi @Strain 3.44 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 132F NC010 Nylon 66
(Unverified Data**) Unreinforced Nucleated Polyamide 66 Zytel 132F NC010 is a nucleated lubricated polyamide 66 for injection molding. It was developed for fast production cycles and high productivity applications.Info.. |