Mechanical Properties Metric English Comments
Tensile Stress 125.68 MPa

@Strain 0.990 %,
Temperature -20.0 °C
18228 psi

@Strain 0.990 %,
Temperature -4.00 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G35HSRX BK099 Nylon 66  (Unverified Data**)
35% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G35HSRX BK099 a 35% glass reinforced heat stabilized hydrolysis resistant PA66 for injection molding. Developed for applications designed fo..