Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 120.82 MPa @Strain 2.59 %, Temperature -20.0 °C |
17523 psi @Strain 2.59 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® HR5315HF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)& 15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5315HF is a 15% glass reinforced PBT with high flow (HF) moderately toughened hydrolysis resistant (HR) resin. Excellen.. |