Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 76.34 MPa @Strain 0.670 %, Temperature 23.0 °C |
11070 psi @Strain 0.670 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® PLS 93G35DH1 BK549 Nylon 6
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 6 Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 76.32 MPa @Strain 4.75 %, Temperature -40.0 °C |
11070 psi @Strain 4.75 %, Temperature -40.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC1010 NC010 Nylon 1010
(Unverified Data**) Unreinforced Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1000 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 90% renewably sourced ingredient by weight. .. |