Mechanical Properties Metric English Comments
Tensile Stress 0.758 MPa

@Strain 100 %
110 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® P3936C TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 0.758 MPa

@Strain 100 %
110 psi

@Strain 100 %
ASTM D412
Teknor Apex Telcar® TL-2635B Thermoplastic Elastomer
Uses: Building Materials; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 100 rpmInformation Provi..
Tensile Stress 0.760 MPa

@Strain 0.000 %,
Temperature 220 °C
110 psi

@Strain 0.000 %,
Temperature 428 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS90G30DR BK099 Nylon 66  (Unverified Data**)
Zytel® PLS90G30DR BK099 is a 30% glass reinforced PA66 nylon resin having superior resistance to hot engine coolant. It is particularly suitable for automotive Radiator End Tanks and other parts in..
Tensile Stress 0.760 MPa

@Strain 0.250 %,
Temperature 90.0 °C
110 psi

@Strain 0.250 %,
Temperature 194 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS LC1610 BK387 Nylon 1010  (Unverified Data**)
Plasticized Toughened Renewably Sourced Polyamide 1010 Developed for Extrusion Information provided by DuPont Performance Polymers