Polymer Property : Tensile Stress = 108.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 108.0 MPa

@Strain 3.40 %,
Temperature 23.0 °C
15660 psi

@Strain 3.40 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 510GR NC000 Acetal (POM)  (Unverified Data**)
10% Glass Reinforced Medium Viscosity Acetal Homopolymer Delrin 510GR is a 10% glass reinforced acetal homopolymer for injection molding. It has high strength stiffness and high deflection temperatu..