Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 10680 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 73.66 MPa

@Strain 1.64 %,
Temperature 23.0 °C
10680 psi

@Strain 1.64 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® HR5315HFS BK591 Polybutylene Terephthalate (PBT)  (Unverified Data**)
15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate with Improved Processing Crastin HR5315HFS is a 15% glass fiber reinforced moderatley toughened hydrolysis resistant polybutylene..
Tensile Stress 73.66 MPa

@Strain 1.64 %,
Temperature 23.0 °C
10680 psi

@Strain 1.64 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® HR5315HFS NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate with Improved Processing Crastin HR5315HFS is a 15% glass fiber reinforced moderatley toughened hydrolysis resistant polybutylene..
Tensile Stress 73.62 MPa

@Strain 0.800 %,
Temperature 0.000 °C
10680 psi

@Strain 0.800 %,
Temperature 32.0 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 74G33W BK196 Nylon 66  (Unverified Data**)
33% Glass Reinforced UV Stabilized Polyamide 66 + Polyamide 6 Zytel 74G33W BK196 is a high gloss automotive weatherable black 33% glass reinforced nylon 66 and nylon 6 comelt resin.Information provi..
Tensile Stress 73.66 MPa

@Strain 0.520 %,
Temperature 23.0 °C
10680 psi

@Strain 0.520 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 92G45DH2 BK083 Polyphthalamide (PPA)
35% Glass Reinforced PPA High Performance Polyamide with DuPont Zytel HTN92G45DH2 BK083 is a 45% glass reinforced high performance polyamide resin using DuPont SHIELD Technology with high flow and e..
Copyright © lookpolymers.com All Rights Reserved