Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 73.26 MPa @Strain 0.650 %, Temperature -20.0 °C |
10630 psi @Strain 0.650 %, Temperature -4.00 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® PLS 93G35DH1 BK549 Nylon 6
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 6 Information provided by DuPont Performance Polymers |