Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 106.06 MPa @Strain 1.00 %, Temperature 0.000 °C |
15383 psi @Strain 1.00 %, Temperature 32.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G33HS1L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G33HS1L NC010 is a 33% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perfor.. |