Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 69.22 MPa @Strain 7.21 %, Temperature 150 °C |
10040 psi @Strain 7.21 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 51G35HSL NC010 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G35HSL NC010 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information .. |
|||
Tensile Stress | 69.19 MPa @Strain 3.60 %, Temperature 150 °C |
10040 psi @Strain 3.60 %, Temperature 302 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 92G35DH2 BK083 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide with DuPont Zytel HTN92G35DH2 BK083 is a 35% glass reinforced high performance polyamide resin using DuPont SHIELD Technology with high flow and e.. |