Polymer Property : Tensile Stress = 10.4 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 10.4 MPa

@Strain 300 %
1510 psi

@Strain 300 %
ISO 37
PolyOne OnFlex™ U 5380A-S0013 Thermoplastic Elastomer (TPE)
OnFlex™-U thermoplastic elastomer compounds are based on thermoplastic polyurethane elastomers (TPE-U). The OnFlex™-U 5300 series are based upon alloys of SEBS and TPU, combining the advantages of..
Tensile Stress 10.4 MPa

@Strain 6.00 %,
Temperature 0.000 °C
1510 psi

@Strain 6.00 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 5553FG NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 10.4 MPa

@Strain 0.250 %,
Temperature 40.0 °C
1510 psi

@Strain 0.250 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK641FR NC010 Polybutylene Terephthalate (PBT)
10% Glass Reinforced Flame Retardant Polybutylene Terephthalate Information provided by DuPont Performance Polymers
Tensile Stress 10.4 MPa

@Strain 10.0 %
1510 psi

@Strain 10.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® HTR4275 BK316 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Hytrel HTR4275 BK316 is designed for blow molding or processing techniques requiring high me..