Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 10.25 MPa @Strain 0.300 %, Temperature 23.0 °C |
1487 psi @Strain 0.300 %, Temperature 73.4 °F |
ISO 11403-1/-2 |
DuPont Performance Polymers Delrin® 511P BK402 Acetal Homopolymer Delrin® 511P is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding(reduced warpage, less shrinkage, fewer voids).Information provided .. |
|||
Tensile Stress | 10.25 MPa @Strain 0.900 %, Temperature 100 °C |
1487 psi @Strain 0.900 %, Temperature 212 °F |
ISO 11403-1/-2 |
DuPont Performance Polymers Delrin® 511P BK402 Acetal Homopolymer Delrin® 511P is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding(reduced warpage, less shrinkage, fewer voids).Information provided .. |