Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 10.08 MPa @Strain 1.19 %, Temperature 40.0 °C |
1462 psi @Strain 1.19 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC1010 NC010 Nylon 1010
(Unverified Data**) Unreinforced Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1000 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 90% renewably sourced ingredient by weight. .. |