Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 1.79 MPa @Strain 100 %, Temperature 23.0 °C |
260 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ OM 1245X-1 Thermoplastic Elastomer (TPE) The Versaflex™ OM 1245X-1 is designed for overmolding onto polycarbonate (PC), ABS, and PC/ABS susbstrates. - Excellent Bond to PC, ABS, PC/ABS - Rubbery Feel - Soft TouchColor concentrates with EV.. |
|||
Tensile Stress | 1.79 MPa @Strain 300 % |
260 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® P2740 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 1.79 MPa @Strain 100 % |
260 psi @Strain 100 % |
|
NEU NeuSoft™ 602-50A Ester TPU / SBC blend |
|||
Tensile Stress | 1.79 MPa @Strain 100 % |
260 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® P1750 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |