Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 1.55 MPa @Strain 300 %, Temperature 23.0 °C |
225 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynalloy™ 8900-30 Thermoplastic Elastomer (TPE) Dynalloy™ 8900-series is an innovative thermoplastic elastomer selection formulated to provide the injection molder with a product capable of overmolding and bonding to both low-density polyethylen.. |