Polymer Property : Tensile Stress = 1.16 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 1.16 MPa

@Strain 100 %
168 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® P1840P TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 1.16 MPa

@Strain 100 %
168 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® P3740 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 1.16 MPa

@Strain 100 %
168 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® P3946 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 1.16 MPa

@Strain 0.0600 %,
Temperature -40.0 °C
168 psi

@Strain 0.0600 %,
Temperature -40.0 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® RS LC1600 BK385 Nylon 1010  (Unverified Data**)
Zytel® RS LC1600 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 60% renewably sourced ingredient by weight. It is flexible, toughened, plasticized, UV and heat stabilized and s..