Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 0.950 MPa @Strain 0.000 %, Temperature 120 °C |
138 psi @Strain 0.000 %, Temperature 248 °F |
50%RH; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS93G35DH1 BK261 Nylon 6
(Unverified Data**) Zytel® PLS93G35DH1 BK261 is a 35% glass reinforced PA6 using SHIELD Technology, only from DuPont, it provides exceptional welding resistance & retention over time thanks to excellent Heat Resistanc.. |
|||
Tensile Stress | 0.950 MPa @Strain 0.0600 %, Temperature -20.0 °C |
138 psi @Strain 0.0600 %, Temperature -4.00 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® RS LC1600 BK385 Nylon 1010
(Unverified Data**) Zytel® RS LC1600 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 60% renewably sourced ingredient by weight. It is flexible, toughened, plasticized, UV and heat stabilized and s.. |