Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 0.7406 MPa @Strain 1.10856 %, Temperature 23.0 °C |
107.4 psi @Strain 1.10856 %, Temperature 73.4 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR237BG BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 45 Shore D Lubricated High Viscosity Polyester Elastomer Developed for Blow Molding Hytrel HTR237BG is designed for blow molding or processing techniques requiring high viscosity. It has nominal dur.. |