Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 0.140 MPa @Strain 300 % |
20.3 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® C4902 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |