Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Total Energy | 65.8 J/cm @Temperature 23.0 °C |
0.123 ft-lb/mil @Temperature 73.4 °F |
Procedure A, C.125; ASTM D4226 |
PolyOne Geon™ Vinyl Rigid Extrusion 87160 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was determined using the notched Izod te.. |