Mechanical Properties Metric English Comments
Dart Drop Total Energy 130 J/cm

@Temperature 23.0 °C
0.244 ft-lb/mil

@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
PolyOne Geon™ Vinyl Rigid Extrusion 87350 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Dart Drop Total Energy 130 J/cm

@Temperature 23.0 °C
0.244 ft-lb/mil

@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
PolyOne Geon™ Vinyl Rigid Extrusion 87850 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne