Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop Total Energy 13.3 J/cm

@Temperature 23.0 °C
0.0249 ft-lb/mil

@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
PolyOne Geon™ HTX Ultra LA427Plus Polyvinyl Chloride Alloy (PVC Alloy)
Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical properties based on Geon HTX Ultra LA427Plus Natural 0000Information provided by PolyOne