Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Total Energy | 89.2 J/cm @Temperature 0.000 °C |
0.167 ft-lb/mil @Temperature 32.0 °F |
ASTM D4226 |
Formosa Plastics Formolon® APW Compound APW Powder Window Profile Compound Series The APW compounds have been designed for profile extrusion in window lineals, fencing and other outdoor weatherable markets. It exhibits excellent whiteness.. |