Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Total Energy | 70.3 J/cm @Temperature 23.0 °C |
0.132 ft-lb/mil @Temperature 73.4 °F |
extruded profile, Procedure A, C.125; ASTM D4226 |
PolyOne Geon™ L4605 Red 7640 Polyvinyl Chloride, Semi-Rigid (PVC, Semi-Rigid) Information provided by PolyOne |