Polymer Property : Dart Drop Total Energy = 0.129 ft-lb/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop Total Energy 68.9 J/cm

@Temperature 23.0 °C
0.129 ft-lb/mil

@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
PolyOne Geon™ HTX E1502 Polyvinyl Chloride Alloy (PVC Alloy)
VSI FLAMMABILITY:Burn Length (0.040 in Bar)ASTM D635 0* IN.Burn Time (0.040 in Bar) ASTM D635 0* Sec.*Extinguished before 25 MM starting ref mark.Information provided by PolyOne