Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Total Energy | 40.5 J/cm @Temperature 0.000 °C |
0.0759 ft-lb/mil @Temperature 32.0 °F |
Procedure A, C.125; ASTM D4226 |
PolyOne Geon™ Vinyl Rigid Extrusion L7801 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Dart Drop Total Energy | 40.5 J/cm @Temperature 0.000 °C |
0.0759 ft-lb/mil @Temperature 32.0 °F |
Procedure B, C.125; ASTM D4226 |
PolyOne Geon™ Vinyl Rigid Extrusion L7801 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |