Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 90.5 GPa @Temperature 93.0 °C |
13100 ksi @Temperature 199 °F |
|
ATI Wah Chang Zircadyne® Alloy Zr 705 Zircadyne 705 is zirconium alloyed with niobium to increase its strength and improve its formability. Alloy exhibits good ductility even at cryogenic temperatures and strength comparable with other .. |