Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | >= 60.0 GPa @Temperature 250 °C |
>= 8700 ksi @Temperature 482 °F |
|
PEAK Werkstoff DISPAL S250 Aluminum Alloy, AlSi20Fe5Ni2, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Modulus of Elasticity | >= 60.0 GPa @Temperature 200 °C |
>= 8700 ksi @Temperature 392 °F |
|
PEAK Werkstoff DISPAL S542 Aluminum Alloy, AlMg6Mn4SiTiZrCo, Condition F Information provided by PEAK Werkstoff GmbH |