Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | >= 58.0 GPa @Temperature 300 °C |
>= 8410 ksi @Temperature 572 °F |
|
PEAK Werkstoff DISPAL S693 Aluminum Alloy, AlCu5Ti, Condition T6 High stiffness and elongation at rupture. Property data for Condition T6 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH |
|||
Modulus of Elasticity | >= 58.0 GPa @Temperature 200 °C |
>= 8410 ksi @Temperature 392 °F |
|
PEAK Werkstoff DISPAL S541 Aluminum Alloy, AlMg6Mn4SiTiZr, Condition F Information provided by PEAK Werkstoff GmbH |