Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 190 GPa @Temperature 399 °C |
27500 ksi @Temperature 750 °F |
|
EDRO #8 Premium 420 Stainless Mold Steel EDRO #8™ is a chromium-alloyed stainless tool steel with the following properties: excellent corrosion resistance, superior polishability, good wear resistance, good machinability, and stability in.. |