Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 185 GPa @Temperature 399 °C |
26800 ksi @Temperature 750 °F |
|
EDRO #3 Prehardened Mold Quality P20 Alloy Steel EDRO #3™ is a vacuum-degassed, ladle refined, Cr-Ni-Mo- alloyed steel which is supplied in the hardened and tempered condition. EDRO #3™ is manufactured to consistently high quality standards with.. |