Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 214 GPa @Temperature -196 °C |
31000 ksi @Temperature -321 °F |
|
Haynes Multimet® alloy, 12.7 mm (1/2 in.) thick plate, 1185°C heat treatment, water quenched Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
Modulus of Elasticity | 214 GPa @Temperature 20.0 °C |
31000 ksi @Temperature 68.0 °F |
Dynamic |
Haynes X-750 Nickel Alloy Sheet and Strip (AMS 5598, UNS N07750) Haynes X-750 (UNS No. N07750) alloy is an age-hardenable, nickel-base superalloy with very good strength at temperatures up to about 1600°F (870°C). It is widely used as a wrought material for.. |
|||
Modulus of Elasticity | 214 GPa @Temperature 20.0 °C |
31100 ksi @Temperature 68.0 °F |
|
EDRO #8 Premium 420 Stainless Mold Steel EDRO #8™ is a chromium-alloyed stainless tool steel with the following properties: excellent corrosion resistance, superior polishability, good wear resistance, good machinability, and stability in.. |
|||
Modulus of Elasticity | 214 GPa @Temperature 100 °C |
31000 ksi @Temperature 212 °F |
|
Bohler-Uddeholm BÖHLER M303 EXTRA Plastic Mold Steel BOHLER M303 EXTRA is a stainless martensitic chromium steel, offering excellent toughness, corrosion and wear resistance. It is characterized by improved machinability and polishability. BOHLER M303.. |