Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 146.8 GPa @Temperature 0.000 °C |
21290 ksi @Temperature 32.0 °F |
|
Special Metals INCOLOY® Alloy 903 A nickel-iron-cobalt alloy with additions of niobium, titanium, and aluminum for precipitation hardening. The alloy combines high strength with a low and constant coefficient of thermal expansion a.. |