Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 208 GPa @Temperature 20.0 °C |
30200 ksi @Temperature 68.0 °F |
Dynamic |
Haynes 625SQ® Nickel Alloy Sheet Haynes 625SQ alloy is a solid-solution strengthened superalloy. It is a modification of Haynes 625 alloy designed to enhance resistance to fatigue at temperatures up to approximately 1200°F (649Â.. |
|||
Modulus of Elasticity | 208 GPa @Temperature 100 °C |
30200 ksi @Temperature 212 °F |
|
Special Metals INCONEL® alloy N06230 Ni-Cr-W-Mo Alloy INCONEL® alloy N06230 (UNS N06230 / W.Nr. 2.4733) is a carbide strengthened nickel-chromium-tungsten-molybdenum alloy with an exceptional combination of strength, stability, and resistance to cor.. |