Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 142 GPa @Temperature 900 °C |
20600 ksi @Temperature 1650 °F |
Dynamic |
Haynes 625SQ® Nickel Alloy Sheet Haynes 625SQ alloy is a solid-solution strengthened superalloy. It is a modification of Haynes 625 alloy designed to enhance resistance to fatigue at temperatures up to approximately 1200°F (649Â.. |